Abstract
X-ray powder data for the compound U3Si have been obtained from an alloy prepared by arc melting uranium and silicon followed by a 7 day anneal at 800°C. The d spacing determinations have been extended into the back reflection to a 2θ value of 167.4 °. The observed relative intensities are compared with calculated values.