Abstract
Metallic Gd1−xCox films (0.75 < × A gives estimates of the uniaxial anisotropy energy Ku. The results indicate that for the composition range studied A increases linearly from 5.7 to 6.6 (10−7 erg/cm), while Ku ranges between 1 and 7 (105 erg/cm3). The saturation magnetization Ms varies between 30 and 180 G. The moderate anisotropy (Q=Ku/2πMs2 = 1–9) and low wall motion coercivity of less than 1 Oe are favorable to bubble device applications. The effect of thermal and magnetic annealing on the magnetic properties is also discussed.