Scale formation on γ-TiAl during oxidation at 800 and 900°C in air and in He + 20% O2
- 1 August 1997
- journal article
- Published by Springer Nature in Oxidation of Metals
- Vol. 48 (1-2), 171-184
- https://doi.org/10.1007/bf01675267
Abstract
No abstract availableKeywords
This publication has 8 references indexed in Scilit:
- Identification of a new phase formed during the oxidation of γ-tttanium aluminumScripta Materialia, 1996
- Studies concerning the effect of nitrogen on the oxidation behavior of TiAl-based intermetallics at 900°COxidation of Metals, 1995
- The effect of nitrogen on the oxidation of γ-TiAlScripta Metallurgica et Materialia, 1995
- The significance of sub-surface depletion layer composition for the oxidation behaviour of γ-titanium aluminidesScripta Metallurgica et Materialia, 1995
- Fundamentals of TiAl oxidation – A critical reviewMaterials and Corrosion, 1995
- Novel phases in the oxidation of γ-titanium aluminumActa Metallurgica et Materialia, 1994
- Kinetics of the α-Fe2O3 formation on Fe3O4 between 400 and 570°C studied by means of X-ray diffraction with grazing incidenceAnalytical and Bioanalytical Chemistry, 1993
- Mechanism of isothermal oxidation of the intel-metallic TiAl and of TiAl alloysOxidation of Metals, 1992