Abstract
Examination of tungsten and tungsten-rhenium samples from TWT helices, using a secondary emission microscope, shows surface defects comparable in size to the skin depth at the operating frequency of the TWT. It is concluded that the difference between measured and calculated helix loss is largely accounted for by these surface defects.