Abstract
We demonstrate formation of an electron-hole liquid in CdS by phase separation of optically excited carriers. Measurement of the electron-hole-liquid density as a function of pump intensity and sample temperature determines the liquid portion of the liquid-gas coexistence curve giving a low-temperature liquid density of 2×1018 cm3 and Tc=55°K.