Failure analysis of a commercially pure titanium plate for osteosynthesis
- 2 December 2002
- journal article
- Published by Elsevier in Engineering Failure Analysis
- Vol. 10 (2), 153-164
- https://doi.org/10.1016/s1350-6307(02)00067-5
Abstract
No abstract availableKeywords
This publication has 24 references indexed in Scilit:
- Failure analysis of surgical implants in BrazilEngineering Failure Analysis, 2002
- Hydrogen in metalsEngineering Failure Analysis, 2001
- AO/ASIF Instruments and ImplantsPublished by Springer Nature ,1994
- The influence of microstructure on the susceptibility of titanium alloys to internal hydrogen embrittlementMetallurgical Transactions A, 1982
- A comparison of gaseous hydrogen embrittlement, slow-strain-rate hydrogen embrittlement, and stress-corrosion cracking InTi-8Ai-1Mo-1VMetallurgical Transactions A, 1981
- Basal and near- basal hydrides in Ti- 5AI- 2.5SnMetallurgical Transactions A, 1978
- A film-rupture model of hydrogen-induced, slow crack growth in acicular alpha-beta titaniumMetallurgical Transactions A, 1976
- Cleavage in Ti-8Al-1Mo-1V caused by hydrogen gasMetallurgical Transactions, 1972
- Environmental hydrogen embrittlement of an α-β titanium alloy: Effect of microstructureMetallurgical Transactions, 1972
- Behavior of hydrogen in α-phase Ti-Al alloysMetallurgical Transactions, 1971