Effects of Sr and Sb modifiers on the sliding wear behavior of A357 alloy under varying pressure and speed conditions
- 20 December 2006
- Vol. 261 (11-12), 1348-1358
- https://doi.org/10.1016/j.wear.2006.03.051
Abstract
No abstract availableThis publication has 22 references indexed in Scilit:
- Effects of Be and Fe on the mechanical and corrosion behaviors of A357 alloysMaterials Chemistry and Physics, 2005
- Plastic deformation behavior of aluminum casting alloys A356/357Metallurgical and Materials Transactions A, 2004
- Correlation between the characteristics of the mechanically mixed layer and wear behaviour of aluminium, Al-7075 alloy and Al-MMCsWear, 2000
- Effects of solution temperature on mechanical properties of 319.0 aluminum casting alloys containing trace berylliumJournal of Materials Research, 2000
- Sliding wear behavior of some Al-Si alloys: Role of shape and size of Si particles and test conditionsMetallurgical and Materials Transactions A, 1998
- Wear of a spray-deposited hypereutectic aluminium-silicon alloyJournal of Materials Processing Technology, 1997
- Effects of be and fe content on plane strain fracture toughness in A357 alloysMetallurgical and Materials Transactions A, 1995
- Effect of magnesium addition and heat treatment on mild wear of hypoeutectic aluminium-silicon alloysActa Metallurgica et Materialia, 1991
- Topographical features observed in a scanning electron microscopy study of aluminium alloy surfaces in sliding wearWear, 1981
- Wear characteristics of as-cast binary aluminium-silicon alloysWear, 1979