The preparation of i n s i t u doped hydrogenated amorphous silicon by homogeneous chemical vapor deposition
- 1 March 1983
- journal article
- research article
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 54 (3), 1461-1465
- https://doi.org/10.1063/1.332172
Abstract
Raman scattering, infrared absorption, conductivity measurements, electron microprobe, and secondary ion mass spectrometry (SIMS) were used to characterize boron and phosphorus doped hydrogenated amorphous silicon (a‐Si:H) films prepared by Homogeneous Chemical Vapor Deposition (HOMOCVD). HOMOCVD is a thermal process which relies upon the gas phase pyrolysis of a source (silane containing up to 1.0% diborane or phosphine) to generate activated species for deposition upon a cooled substrate. Doped films prepared at 275 °C by this process were found to contain ∼12‐at. % hydrogen as determined by infrared absorption. We examined dopant incorporation from the gas phase, obtaining values for a distribution coefficient CD (film dopant content/gas phase dopant concentration, atomic basis) of 0.33≤CD ≤0.63 for boron, while 0.4≤CD ≤10.75 in the limits 3.3×10−5≤PH3/SiH4≤0.004. We interpret the data as indicative of the formation of an unstable phosphorus/silicon intermediate in the gas phase, leading to the observed enhancements in CD at high gas phase phosphine content. HOMOCVD films doped at least as efficiently as their prepared counterparts, but tended to achieve higher conductivities [σ≥0.1 (Ω cm)−1 for 4.0% incorporated phosphorus] in the limit of heavy doping. Raman spectra showed no evidence of crystallinity in the doped films. Film properties (conductivity, activation energy of of conduction) have not saturated at the doping levels investigated here, making the attainment of higher ‘‘active’’ dopant levels a possibility. We attribute the observation that HOMOCVD appears more amenable to high ‘‘active’’ dopant levels than plasma techniques to the low (∼0.1 eV) thermal energy at which HOMOCVD proceeds, versus ∼10–100 eV for plasma techniques. Low substrate temperature (75 °C) doped films were prepared with initial results showing these films to dope as readily as those prepared at high temperature (T∼275 °C).Keywords
This publication has 20 references indexed in Scilit:
- Doping effects on post-hydrogenated chemical-vapour-deposited amorphous siliconPhilosophical Magazine Part B, 1982
- The role of hydrogen in heavily doped amorphous siliconPhilosophical Magazine Part B, 1982
- Preparation of amorphous silicon films by chemical vapor deposition from higher silanes SinH2n+2(n≳1)Applied Physics Letters, 1981
- Preparations of a-Si:H from Higher Silanes (SinH2n+2) with the High Growth RateJapanese Journal of Applied Physics, 1981
- Low pressure deposition of polycrystalline silicon from silaneJournal of Crystal Growth, 1981
- Kinetics and mechanism of amorphous hydrogenated silicon growth by homogeneous chemical vapor depositionApplied Physics Letters, 1981
- Hydrogenated amorphous-silicon thin films produced by ion platingApplied Physics Letters, 1980
- Low Pressure Silicon EpitaxyJournal of the Electrochemical Society, 1977
- Doping, Schottky barrier and pn junction formation in amorphous germanium and silicon by rf sputteringSolid State Communications, 1976
- Electronic properties of substitutionally doped amorphous Si and GePhilosophical Magazine, 1976